Titanium alloys are divided into alpha alloys, near-alpha alloys, alpha and beta alloys, and beta alloys. Grade Ti 15V 3Cr 3Al 3Sn alloy is a beta alloy that can be strip-rolled and heat-treated. It is highly formable, and has good room temperature bending properties. Solution treatment of this alloy enhances its strength.
Standard |
Werkstoff No. |
UNS |
Titanium Alloy Ti 15V-3Cr-3Sn-3Al (Ti 15333) |
|
R58153 |
Technical Data Sheet
Chemical Composition |
|||||||||||
Weight % |
Ti |
Al |
Sn |
Cr |
V |
C |
Fe |
N |
O |
H |
|
Titanium Alloy Ti 15V-3Cr-3Sn-3Al (Ti 15333) |
Balance |
2.5~3.5 |
2.5~3.5 |
2.5~3.5 |
14~16 |
0.08 |
0.3 |
0.03 |
0.15 |
0.015 |
Typical Mechanical Properties (Tensile Requirements)
Material |
Tensile Strength, min |
Yield Strength (0.2% Offset) min or range |
Elongation in 4D,min% |
||
ksi |
MPa |
ksi |
MPa |
||
Titanium Alloy Ti 15V-3Cr-3Sn-3Al (Ti 15333) |
145 |
1000 |
140 |
966 |
7 |
Titanium Alloy Grade5 Ti-6Al-4V alloy is the most widely used titanium alloy of the alpha-plus-beta class, and is also the most common of all titanium alloys. The alloy is castable and is u
Titanium Alloy Grade4 is “unalloyed” titanium offering optimum ductility and cold formability. The material has high impact toughness and is readily weldable. The material is capable o
Titanium Alloy Grade 3 is “unalloyed” titanium offering improved strength,moderate ductility, and ASME Code design allowable. The material is readily weldable. This material is very corrosion re
Titanium Alloy Grade 2 is “unalloyed” titanium offering an excellent balance of strength and ductility. The material has good toughness and is readily weldable. This material is very corrosion r