Titanium Grade 12 is similar to Grade 2 and Grade 3 except Grade 12 has the addition of Mo and Ni. These additions to Grade 12 offer a lower cost option than the Palladium bearing grades. Grade 12 has high strength, good heat and wear resistance and is highly weldable. Grade 12 is used for Chemical Processing, Power generation, Desalination, Marine Hydrocarbon processing and Mining.
Standard Specification:
Standard |
Werkstoff No. |
UNS |
Titanium Alloy Grade 12 Ti-0.3Mo-0.8Ni |
3.7105 |
R53400 |
Technical Data Sheet
Chemical Composition |
||||||||||||
Weight % |
Ti |
Ni |
Mo |
C |
Fe |
N |
O |
H |
||||
Titanium Alloy Grade 12 Ti-0.3Mo-0.8Ni |
Balance |
0.6/0.9 |
0.2/0.4 |
0.08 |
0.3 |
0.03 |
0.25 |
0.015 |
Typical Mechanical Properties (Tensile Requirements)
Material |
Tensile Strength, min |
Yield Strength (0.2% Offset) min or range |
Elongation in 4D,min% |
Reduction of Area Min % |
||
ksi |
MPa |
ksi |
MPa |
|||
Titanium Alloy Grade9 Ti-3Al-2.5V |
70 |
483 |
50 |
345 |
18 |
25 |
Titanium 6-2-4-2 (6Al-2Sn-4Zr-2Mo) is an alpha-beta titanium alloy capable of being heat treated to higher strengths in greater section sizes that 6Al-4V. Widely used in forged components, 6-2-4-2 bet
Ti-6Al-4V alloy is the most widely used titanium alloy of the alpha-plus beta class, and is also the most common of all titanium alloys. This modification incorporates extra low interst
Titanium Alloy Grade5 Ti-6Al-4V alloy is the most widely used titanium alloy of the alpha-plus-beta class, and is also the most common of all titanium alloys. The alloy is castable and is ut